石油压裂砂:
该砂是一种纯天然石英砂,经水洗、脱泥、颗粒筛分后烘干,颗粒圆整、粒度均匀、表面光洁、流动性好、具有较高的抗破碎度,是油田采油用最理想的压裂支撑剂.
压裂砂主要物化性能
筛目 |
粒经 |
SIO2 |
结构 |
粘土及细 |
破碎率 |
浊度 |
酸溶度 |
视密度 |
体密度 |
圆球度 |
/cm² |
mm |
颗粒含量 |
80 Mpa |
NTU |
% |
g/cm3 |
g/cm3 |
20 |
0.9 |
≥96 |
单晶粒 |
≤0.01 |
≤0.02 |
≤50 |
≤2.0 |
>1400 |
>2.5 |
≥0.6 |
24 |
0.8 |
≥96 |
单晶粒 |
≤0.01 |
≤0.02 |
≤50 |
≤2.0 |
>1400 |
>2.5 |
≥0.6 |
28 |
0.63 |
≥96 |
单晶粒 |
≤0.01 |
≤0.02 |
≤50 |
≤2.0 |
>1400 |
>2.5 |
≥0.6 |
35 |
0.5 |
≥96 |
单晶粒 |
≤0.01 |
≤0.02 |
≤50 |
≤2.0 |
>1400 |
>2.5 |
≥0.6 |
45 |
0.4 |
≥96 |
单晶粒 |
≤0.01 |
≤0.02 |
≤50 |
≤2.0 |
>1400 |
>2.5 |
≥0.6 |
50 |
0.355 |
≥96 |
单晶粒 |
≤0.01 |
≤0.02 |
≤50 |
≤2.0 |
>1400 |
>2.5 |
≥0.6 |
28 |
0.63 |
≥96 |
单晶粒 |
≤0.01 |
≤0.02 |
≤50 |
≤2.0 |
>1400 |
>2.5 |
≥0.6 |
30 |
0.6 |
≥96 |
单晶粒 |
≤0.01 |
≤0.02 |
≤50 |
≤2.0 |
>1400 |
>2.5 |
≥0.6 |
40 |
0.45 |
≥96 |
单晶粒 |
≤0.01 |
≤0.02 |
≤50 |
≤2.0 |
>1400 |
>2.5 |
≥0.6 |
50 |
0.355 |
≥96 |
单晶粒 |
≤0.01 |
≤0.02 |
≤50 |
≤2.0 |
>1400 |
>2.5 |
≥0.6 |
60 |
0.3 |
≥96 |
单晶粒 |
≤0.01 |
≤0.02 |
≤50 |
≤2.0 |
>1400 |
>2.5 |
≥0.6 |
70 |
0.22 |
≥96 |
单晶粒 |
≤0.01 |
≤0.02 |
≤50 |
≤2.0 |
>1400 |
>2.5 |
≥0.6 |
产品检验依据标准:
SY5184-1997 油、气、水井防砂作业用石英砂标准
SY/T5108-1997 石油、天然气行业标准、压裂支撑剂性能测试方法。
|
 |
|